Insights · Materials
6061 vs 6082 vs 7075 vs 2014: Choosing an Aluminum Alloy for Forged Parts
·3 min read

Most aluminum forgings are made from four alloys: 6061, 6082, 7075 and 2014. The 6xxx alloys are the all-round choice: good strength, very good corrosion resistance and easy anodizing. 7075 and 2014 are chosen when a part must be as strong and light as possible, and accept lower corrosion resistance in return.
This guide compares the four alloys in the T6 condition (solution heat treated and artificially aged), the usual temper for forged aluminum parts.
Quick comparison
| Alloy (T6) | Tensile strength, typical | Yield strength, typical | Corrosion resistance | Anodizing | Weldability |
|---|---|---|---|---|---|
| 6061 | about 310 MPa | about 275 MPa | Very good | Very good | Good |
| 6082 | about 310–340 MPa | about 260–310 MPa | Very good | Very good | Good |
| 7075 | about 570 MPa | about 500 MPa | Moderate | Good (hard anodizing) | Poor |
| 2014 | about 480 MPa | about 410 MPa | Low; needs protection | Fair | Poor |
The figures are typical values from published alloy datasheets, for comparison only. Guaranteed minimum values depend on the standard, the temper and the section thickness of the forging, so always specify them on the drawing.
6061: the general-purpose forging alloy
6061 is the most widely used heat-treatable aluminum alloy in North America. It forges well, machines cleanly after T6 heat treatment and takes decorative or hard anodizing in any color.
Typical forged parts: brake calipers, bicycle hub shells, motorcycle triple clamps, scroll compressor components and other machined parts where good strength, a clean anodized finish and corrosion resistance are all needed.
6082: the European equivalent, slightly stronger
6082 (EN AW-6082) is the European counterpart of 6061 and the most common structural alloy in Europe. It is usually a little stronger than 6061 and has the same very good corrosion resistance, which makes it the standard choice for parts exposed to water and outdoor use.
Typical forged parts: Storz and fire hose couplings, blank caps, hose safety clamps and horse racing plates.
7075: maximum strength for light, load-bearing parts
7075 (EN AW-7075) is a zinc-alloyed aluminum and one of the strongest aluminum alloys: in the T6 condition it is close to the strength of many mild steels at about a third of the weight. It is harder to forge than 6xxx alloys, needs careful temperature control, and has lower corrosion resistance, so parts are normally hard anodized.
Typical forged parts: climbing and rescue carabiners, figure-8 descenders, high-performance connecting rods, bicycle hubs and motorcycle triple clamps.
2014 (2A14): strength at high temperature
2014 is a copper-alloyed aluminum. It keeps its strength better than 6xxx alloys at elevated temperatures and is forged for parts that run hot or at high speed. Its corrosion resistance is the lowest of the four, so parts are usually protected by coating or anodizing.
Typical forged parts: turbocharger compressor wheels and other rotating parts. The Chinese grade 2A14 is the equivalent of AA 2014.
Grade equivalents
| ASTM / AA | EN (DIN EN 573-3) | China (GB/T 3190) |
|---|---|---|
| 6061 | EN AW-6061 | 6061 |
| 6082 | EN AW-6082 | 6082 |
| 7075 | EN AW-7075 | 7075 (7A09 is a similar grade) |
| 2014 | EN AW-2014 | 2A14 |
| 2024 | EN AW-2024 | 2A12 |
How to choose
- Outdoor, wet or marine use, anodized finish: 6082 or 6061.
- Highest strength-to-weight, safety-critical parts: 7075-T6, hard anodized.
- Rotating or hot-running parts: 2014 (2A14).
- Parts that must be welded after forging: a 6xxx alloy; 7075 and 2014 are not normally welded.
- Cost: 6xxx alloys are generally the lowest-cost choice and the easiest to forge and machine.
FAQ
Is 7075 always better than 6061? No. 7075 is much stronger, but 6061 resists corrosion better, anodizes more evenly and costs less. Choose 7075 only when the strength is needed.
Is 6082 the same as 6061? They are close equivalents and often interchangeable. 6082 is common in Europe and usually a little stronger; 6061 is common in North America and Asia.
Which aluminum alloys does Aviaforge forge? Mainly 6061, 6082, 6063, 7075, 5083, 2024 and 2A14 (2014), plus carbon and alloy steels such as C45 and 42CrMo4, to ASTM, DIN EN and GB standards. See our forging capabilities or send us your drawing for an alloy recommendation.